Chemical name Ethyl silicate 40
Structural Formula 

1.png

Property Degree of polymerzation (DP) :n=4-5
CAS NO.:11099-06-2
SiO2 content(%) :40.0-42.0
Relative Density d420 °C :1.04-1.07
Acid (HCl)% :≤0.1
Volatile components(under110°C) :≤3
Appearance: Colorless transparent liquid.
Dissovability: Soluble in most organic solvents.
Application Adhesion promoter for paints &coatings, precision casting materials and ceramic materials; silicone rubber cross-linking agent.