Description:


Chemical Name:3-Mercaptopropyltriethoxysilane
Molecular Formula:C9H22O3SSi
Structural Formula:590.png
Molecular Weight:238.42 
CAS No.:14814-09-6


Physical Properties


Physical Form:Transparent liquid

Color:Light yellow

Specific Gravity at 25/25℃:0.993

Boiling Point,℃:210

Refractive Index, nD 25℃:1.4331

Flash Point, Pensky-Martens Closed Cup(1),℃:88


Applications


It is mainly used with inorganic fillers including carbon black, SiO2, etc. It has the function of activating, coupling, crosslinking and reinforcing in polymers, such as rubber, silicone rubber, etc. Also, it has functions similar as KH-580.  

                                   